Search
Search
Primary XPS region: Pt4f
Overlapping regions: Al2p
Binding energies of common chemical states:
| Chemical state | Binding energy Pt4f7/2/eV |
|---|---|
| Pt metal | 71.0 |
| PtO | 72.4 |
| PtO2 | 74.9 |
About This ElementSymbol: Pt
Date of Discovery: 1735
Name Origin: Spanish platina
Appearance: silver
Discoverer: Julius Scaliger
Obtained From: platinum ores
Melting Point: 2041 K
Boiling Point: 4098 K
Density[kg/m3]: 21090
Molar Volume: 9.09 × 10-6 m3/mol
Protons/Electrons: 78
Neutrons: 117
Shell Structure: 2,8,18,32,17,1
Electron Configuration: [Xe]4f145d96s1
Oxidation State: 2,4
Crystal Structure: cubic
Discovered by J. Scaliger in 1735, platinum is
a beautiful gray-white metal that is malleable
in its pure form. It is extremely resistant to corrosion and tarnishing, and will not oxidize in air, even at high temperature. Platinum is very rare, and is naturally found as the uncombined metal. Because of its extreme durability and resistance to tarnishing, platinum is widely used to make jewelry. It is also used to make surgical tools, liquid crystal displays, and electrical resistance wires. Platinum is named for the Spanish word “platina,” meaning “little silver.”